dc.contributor.authorAL DHUBAIBI, Ammar mahdi
dc.contributor.authorVapur, Hüseyin
dc.contributor.authorTop, Soner
dc.date.accessioned2023-11-23T08:19:38Z
dc.date.available2023-11-23T08:19:38Z
dc.date.issued2019en_US
dc.identifier.issn2149-2123
dc.identifier.issn2148-4171
dc.identifier.urihttp://doi.org/10.17350/HJSE19030000148
dc.identifier.urihttps://hdl.handle.net/20.500.12573/1844
dc.descriptionThis study was supported by Department of Scientific Research Projects, Cukurova University, (Project No: FLY-2019-11823)en_US
dc.description.abstractThe aim of this study was to obtain a high grade and yield percentage of iron concentratefrom a specularite ore by using wet magnetic separation and reverse flotation techniques.The processing a specularite sample using wet magnetic separation and reverseflotation method was studied. During the magnetic separation process, particle size was-2000 μm and magnetic field applied at 0.25 T and 0.85 T which were performed at asolid-liquid ratio of 10% and 20% by weight, respectively. In the reverse flotation tests,experimental design (DOE) was applied, statistically. Depressant dosage, collector dosageand flotation time were selected as main parameters. PH value, frother dosage (MIBC) andparticle size were constant parameters. The results showed that particle size and magnetic fieldintensity had a significant effect on the iron concentrate grade and yield for wet magneticseparation. The optimum value of iron concentrate grade was 98.75% at 0.25 T andparticle size of -150 μm while the highest value of iron concentrate yield was 67% at 0.75T and particle size of -74 μm. In the flotation tests, depressant dosage had the greatestinfluence on the iron concentrate grade while the effect of the collector dosage and frothcollection time were less. Froth collection time had the greatest effect on iron concentrateyield.The maximum iron concentrate grade was 90.13% for the following conditions:5250 g/ton depressant, 1000 g/ton collector and 2-minute froth collection time. Themaximum iron concentrate yield was 98.96% for the following conditions: 5250 g/tondepressant, 1500 g/ton collector and 1 min froth collection time under fixed conditions.en_US
dc.language.isoengen_US
dc.publisherHİTİT ÜNİVERSİTESİen_US
dc.relation.isversionof10.17350/HJSE19030000148en_US
dc.rightsinfo:eu-repo/semantics/openAccessen_US
dc.subjectMagnetic separationen_US
dc.subjectReverse flotationen_US
dc.subjectParticle sizeen_US
dc.subjectUpgradingen_US
dc.subjectSpeculariteen_US
dc.subjectExperimental designen_US
dc.titleEffective Processing of Specularite Ore by Wet Magnetic Separation and Reverse Flotation Techniquesen_US
dc.typearticleen_US
dc.contributor.departmentAGÜ, Mühendislik Fakültesi, Malzeme Bilimi ve Nanoteknoloji Mühendisliği Bölümüen_US
dc.contributor.authorID0000-0003-3486-4184en_US
dc.contributor.institutionauthorTop, Soner
dc.identifier.volume6en_US
dc.identifier.issue3en_US
dc.identifier.startpage201en_US
dc.identifier.endpage208en_US
dc.relation.journalHittite Journal of Science and Engineeringen_US
dc.relation.publicationcategoryMakale - Ulusal Hakemli Dergi - Kurum Öğretim Elemanıen_US